Pinhole
|
1. Spraying air pressure is too low
2. A large amount of paint 3. A thicker film. |
1. Adjustment of air pressure
2. Control the film thickness
3.To increase the dissolution power of thin material |
|
Sagging
|
1. A large amount of paint
2.Construction of the viscosity is too low 3. Dilute volatile material slowly 4.Environmental emperature at the end of the low one |
1.Adjustment; spraying conditions
2. For quick drying of thin materials |
|
Flooding
|
1. A large amount of paint
2. Construction of the viscosity is too low 3. Ambient temperature lower one. |
1.Adjustment; spraying conditions
2. For quick drying of thin materials |
|
Orange peel
|
1. Out of a small amount of paint
2. GUN far away from 3. High temperature 4. Dilute volatile material fast one. |
1.Adjustment; spraying conditions
2. For slow drying thinner |
|
Exposed at the end of one.
|
1. Construction of the viscosity is too low
2. Film thickness of |
1. Improve the construction viscosity
2. Increase the film thickness |
|
Pale one.
|
1.Air humidity
2. A high temperature. |
1.Plus anti-white-agent
|
|
Bite at the end of one.
|
1.Construction of the viscosity is too low
2. Dilute power is too strong a material dissolved. |
1. Improve the construction viscosity
2. For dissolving power is low for thin material |
|
A high luster.
|
1.Spraying high viscosity
2. Film thickness 3. Dilute volatile material slowly 4. A large amount of paint 5. A high-gloss paint. |
1.Reduce the spraying viscosity
2. Control the film thickness 3. Adjustment of spray 4. Injecting matting agent |
|
Particle
|
1. Substrates untreated clean
2. Paints a particle 3. Air impurities |
1. Deal with the substrate
2. With the appropriate filter, paint 3. Air Filter |
|
Diaoqi
|
1. Substrates untreated clean
2. Construction of the viscosity is too high 3. Dilute power is too weak material dissolved 4. Paint itself is a poor attachment. |
1. Deal with the substrate
2. Adjusting the construction viscosity 3. For use of highly dilute dissolved material 4. Adjustment of coating formulations |
Copyright © 2002-2007 Shenzhen Ci Cai Chemical Technology Co., Ltd.
WebSite:www.szcicai.com Customer Service:86-0755-28436558