Home > Questions
|
Problems
|
Analysis
|
Solution
|
|
Finish off a bad adhesion.
|
1.Solvent evaporation is not complete
2. Primer contaminated 3. Solidification incomplete 4. Paint is not supporting one. |
1. Improve the leveling of temperature and time, reduce film thickness
2. After the primer coating material to keep clean, do not touch hand 3. Check-curing equipment is properly 4. Replacement Topcoat |
|
Even at the end off a bad adhesion.
|
1.Primer attached to poor
2. Topcoat to bite at the end of one. |
1.Adjustment or replacement of primer
2. Paint and primer do not match, use the same factory matching paint |
|
Particles, Ma points
|
1. In the air more dust, impurities
2. Paint contaminated one. |
1.Clean Air
2. With 500 mesh filter, paint |
|
Hardness bad one.
|
1.Energy is too low, curing is not fully
2. Paint is not supporting 3. Painting itself is a somewhat less hardness. |
1.Adjust the curing energy
2. Supporting the use of coating 3. Adjust the coating formulation |
|
From shrinkage, a crater.
|
1.Primer contaminated
2. Compressed air contamination 3. Contaminated paint 4. Spray gun, spray pipe pollution |
1. Replacement of contaminated paint
2. Check the oil-water separator 3. Adding some shrink holes in the paint additive 4. Clean spray gun, pipe |